description:
SPECIFICATIONS
Type core
Design
Diameter, mm
Protective environment
Welding current
The position of the seam
Carbonate-fluorenyl
Tubular
1,6; 2,0; 2,4
s/s
=+
Downhand
TYPICAL CHEMICAL COMPOSITION of DEPOSITED METAL, %
C
Mn
Si
Al
S
P
≤ 0,15
1,0 - 1,5
0,2 - 0,5
0,8 - 1,0
≤ 0,03
≤ 0,03
THE MECHANICAL PROPERTIES OF THE WELD METAL
σt, MPa |
σy, MPa |
δ,% |
An,J/sm2(+20oС) |
---|---|---|---|
500 - 650 |
≥ 440 |
≥ 20 |
≥ 80 |
MODES OF WELDING-CORED WIRE
Diameter, mm | Iсв,А | Uд,В | Extension, mm |
---|---|---|---|
1,6 |
150 - 280 | 22 - 24 | 25 - 35 |
2,0 |
200 - 350 |
22 - 26 | 25 - 35 |
2,4 |
250 - 450 |
26 - 28 | 25 - 35 |
The developed method of welding allows to obtain high-quality welds, including welding in installation and field conditions.